For magnetic materials. The samples should be electrolytically polished. To prepare a colloidal Fe3O4 suspension, solution A is heated to 30-40°C and mixed with solution B while stirring vigorously. Fe3O4 is filtered and mixed several times with dist. water several times. 1 ml Fe3O4 is mixed with 30 ml 0.3% soap solution. 1 drop of the suspension is placed on the surface of the sample and covered with a cover glass. The treated sample is observed in the bright field or dark field of an incident light microscope. The Fe3O4 - particles decorate the domain walls because of the uneven magnetic field there.

Article no.: 18979

Etchant for magnetic materials

  •   Container size and order number Net price Amount
    KIT: Bitter Technique (Etchant) - 100 ml
    Order number: 18979.00100
    17,47 €
    KIT: Bitter Technique (Etchant) - 250 ml
    Order number: 18979.00250
    20,13 €
    KIT: Bitter Technique (Etchant) - 500 ml
    Order number: 18979.00500
    18,94 €
    KIT: Bitter Technique (Etchant) - 1.000 ml
    Order number: 18979.01000
    35,62 €
    KIT: Bitter Technique (Etchant) - 2.500 ml
    Order number: 18979.02500
    66,41 €

Important Information

Warning labels:

Lagerung: 15 … 25 °C

Haltbarkeit: 24 Monate

product information

Relevant Incredients:
• Iron(III) Chloride 40 %
• Sodium hydroxide
• Iron (II) chloride tetrahydrate